Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 33.5 MPa | 4860 psi | ASTM D638 |
Owens Corning Glass Fiber Reinforced Polyester BMC (Injection), 22 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |