Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.100 - 0.230 MPa | 14.5 - 33.4 psi | ASTM D3574E |
Covestro Bayfit® High Density Polyurethane Flexible Molded Foam, High Density Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |