Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2230 MPa | 324000 psi | |
Latrobe 440â„¢ N-DUR High Quality Martensitic Stainless Steel 440 N-DUR is a 15.0% chromium stainless steel that provides the corrosion resistance of 440 C with the added benefit of improved carbide size and distribution for noiseless miniature precision beari.. |