Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 3100 MPa | 450000 psi | |
China Tungsten YG15C Tungsten Carbide Information provided by China Tungsten |
|||
Tensile Strength, Ultimate | 3100 MPa | 450000 psi | |
China Tungsten YG13 Tungsten Carbide Information provided by China Tungsten |
|||
Tensile Strength, Ultimate | 3100 MPa @Thickness 25.4 mm |
450000 psi @Thickness 1.00 in |
filament |
3M Nextel™ 610 Composite Ceramic Fiber Chemical composition above is wt%. Filament diameter is 10-12 µm.3M Nextel Ceramic Fibers 610, 650, and 720 are composite grade fibers. They have a refined crystal structure based on alpha-Al2O3 .. |