Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 31.72 MPa | 4601 psi | Tensile tester jaw separation 10 in/min (25.4 cm/min). Typical properties based on film cast from toluene solution.; ASTM D412 |
Kraton® D1102 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Tensile Strength, Ultimate | 31.72 MPa | 4601 psi | Tensile tester jaw separation 10 in/min (25.4 cm/min). Typical properties based on film cast from toluene solution.; ASTM D412 |
Kraton® D1116 (SB)n Branched Copolymer (SB)n - styrene-butadiene multi-arm (branched) copolymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve .. |
|||
Tensile Strength, Ultimate | 31.72 MPa | 4601 psi | Tensile tester jaw separation 10 in/min (25.4 cm/min). Typical properties based on film cast from toluene solution.; ASTM D412 |
Kraton® D1101 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |