Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 21.0 MPa | 3040 psi | ISO 527-1 |
Polikim ULPOLEN® 1000 UHMWPE, Oil The solid lubricant additive reduces Ulpolen®'s coefficient of friction even further. As the additive is dry, it does not accumulate dust or dirt. In conveyor belts, it reduces squeakings at corner.. |