Polymer Property : Tensile Strength, Ultimate = 3.716 MPa
Polymer Property :
Tensile Strength, Ultimate =
3.716 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
>=
3.716
MPa
>=
538.9
psi
Fujipoly Industries FLAT-5TV-10-.75 silicone rubber fusible tape
Information provided by Fujipoly Industries