Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 296 MPa @Temperature 871 °C |
43000 psi @Temperature 1600 °F |
|
Universal Wire Works 617 Nickel Alloy Welding Wire Alloy 617 is used for TIG and MIG welding of Inconel type alloy 617 and alloys of similar composition. Alloy 617 welds produce high stress-rupture strength in prolonged exposure to high temperatures.. |
|||
Tensile Strength, Ultimate | 296 - 359 MPa | 43000 - 52000 psi | |
Eagle Brass 110 EPT COPPER, Hard Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Strength, Ultimate | 296 - 352 MPa | 43000 - 51000 psi | |
Eagle Brass 151 ZHC® COPPER, 1/2 Hard Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Tensile Strength, Ultimate | 296 - 345 MPa | 43000 - 50000 psi | |
Eagle Brass 706 Copper Nickel 10%, Annealed 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Tensile Strength, Ultimate | 296 - 359 MPa | 43000 - 52000 psi | |
Eagle Brass 101 OFE COPPER (Certified), Hard Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Ultimate | 296 - 359 MPa | 43000 - 52000 psi | |
Eagle Brass 102 OF COPPER (Non-Certified), Hard Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Strength, Ultimate | 296 MPa | 42900 psi | |
AK Steel Cold Rolled Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade Interstitial Free (I-F) steels are made by adding titanium and/or niobium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel |
|||
Tensile Strength, Ultimate | >= 296 MPa | >= 42900 psi | |
AK Steel ZINCGRIP® ELECTRASMOOTH® Electrogalvanized Carbon Steel, Bake Hardenable (BH 180) Brake Hardenable steels offer good formability and an increase in strength after paint bake.Information provided by AK Steel |
|||
Tensile Strength, Ultimate | 296 MPa | 42900 psi | Typical |
Alpase M-1™ Aluminum Mold Plate M-1™ features and benefits include: Dimensional stability, fully weldable, anodizable, consistent hardness - regardless of size, can be nickel plated, good machinability, no heat treatment required.. |