Tensile Strength, Ultimate 20.3 MPa
2950 psi
Sylvin Technologies 9604-90 Clear PVC for Injection Molding
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 20.3 MPa
2950 psi
ASTM D412
Colorite Polymers CS6038SR Wire and Cable Insulation Vinyl Compound
Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai..