Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 10.9006 - 29.9646 MPa @Temperature 100 - 100 °C |
1581.00 - 4346.01 psi @Temperature 212 - 212 °F |
Average value: 23.0 MPa Grade Count:11 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |
|||
Tensile Strength, Ultimate | 10.9006 - 29.9646 MPa @Time 252000 - 3.60e+6 sec |
1581.00 - 4346.01 psi @Time 70.0 - 1000 hour |
Average value: 23.0 MPa Grade Count:11 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |