Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 193.1 MPa
28010 psi
ASTM D638
PTS Trimid® N66-G43HL 43% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength, Ultimate 193.1 MPa
28010 psi
ASTM D638
PTS Trimid® N66-G43L 43% Glass Fiber Reinforced Lubricated Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).