Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 28.1 MPa | 4080 psi | 0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638 |
Americas Styrenics STYRON™ A-TECH™ 1220 High-Impact Polystyrene Resin
(discontinued **) STYRON™ A-TECH™ 1220 advanced technology polystyrene resin is a high impact, high modulus resin for extrusion thermoforming applications. The improved durability of this resin allows potential do.. |
|||
Tensile Strength, Ultimate | 28.1 MPa | 4080 psi | 150°C, 40 min., Pressure Vulcanization. -8% Change after 100°C, 70 hrs, Oil Immersion |
KKPC KOSYN KNB 25M Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |
|||
Tensile Strength, Ultimate | 28.1 MPa | 4080 psi | |
Williams Advanced Alloys WS238A Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |