Polymer Property : Tensile Strength, Ultimate = 2725 psi
Polymer Property :
Tensile Strength, Ultimate =
2725 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
18.79
MPa
2725
psi
Sylvin Technologies 8940-95 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.