Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 27.901 MPa | 4046.7 psi | |
BCC Products MB 8250 Aluminum Board MB 8250 is an aluminum filled product that is dimensionally stable and exhibits great machinable properties. Features: excellent machineability, low dust emission, no shrinkage, low moisture absorp.. |