Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1828 MPa | 265100 psi | |
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition CH 900 AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala.. |