Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 18.3 MPa | 2650 psi | ASTM D638-95 |
Multibase Multi-Pro® 5002 X White 50% Filler Content Polypropylene Multi-Pro 5002 X White is an extrusion grade filled polypropylene that has good stiffness as well as excellent impact properties. It can be made in any color.Data provided by Multibase. |
|||
Tensile Strength, Ultimate | 18.3 MPa | 2650 psi | 500 mm/min (20 in./min.); ASTM D638, Type IV Specimen |
Eastman M3007-P Polyethylene
(discontinued **) M3007-P is suggested for applications such as spiral-wound can linings, release paper, and photographic paper. M3007-P Has been found to exhibit good barrier properties, temperature resistance, and.. |
|||
Tensile Strength, Ultimate | 18.3 MPa | 2650 psi | ASTM D412 |
Multibase Multi-Flex® RP 6568 B2 Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Ultimate | 18.3 MPa | 2650 psi | |
Sylvin Technologies 8950-95 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 18.3 MPa | 2650 psi | |
Sylvin Technologies 9600-90 Clear PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Tensile Strength, Ultimate | 18.3 MPa | 2650 psi | Molded property |
Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2037 Polyethylene is a cast film extrusion resin for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a when used unmodified and according to good.. |
|||
Tensile Strength, Ultimate | 18.3 MPa | 2650 psi | ASTM D412 |
Colorite Polymers CS904015 Wire and Cable Jacket Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Tensile Strength, Ultimate | 18.3 MPa | 2650 psi | Cured 7 min at 177°C and Post Cured 2 hr at 232°C |
DuPont Performance Polymers VTR 8550 (GFLT-S) Peroxide Cured Fluoroelastomer (FKM) Formulation
(discontinued FormulationVTR-8550 |