Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 18.20 MPa | 2639 psi | ASTM D638 |
Colorite Polymers 8566 Non-Phthalate 66 Series Vinyl Compound Description: The Colorite 66 series is a family of non-toxic PVC compounds developed specifically for those medical device, food, and infant care items for which the use of a citrate* based non-phth.. |