Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 26.8 MPa | 3880 psi | ASTM D638 |
Multibase Nylex™ 1404 NAT Polyamide + PP Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing.. |