Polymer Property : Tensile Strength, Ultimate = 249 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1.38 - 1.72 MPa
200 - 249 psi
ASTM D412
BASF Master Builders Solutions ChemRex® CX-25 Polyurethane Adhesive/Sealant  (discontinued **)
CX-25 is a polyurethane based one-component, moisture curing adhesive/sealant. It provides fast cure, non-sag, excellent adhesion and has elastomeric properties with high strength which can reduce/..