Polymer Property : Tensile Strength, Ultimate = 2412 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 16.63 MPa
2412 psi
ASTM D638
Ecomass® 3800ZD82 Tungsten Filled Polymethylpentene
Nontoxic alternative to Lead (Pb), radiation shielding applicationsModerate Specific GravityTungsten Powder Filled Polymethylpentene (TPX)RigidInformation provided by Technical Polymers