Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 166 MPa | 24100 psi | ATSM D638 |
Ashley Polymers Ashlene® 528L-25G Nylon 66, 25% Glass Reinforced General purpose glass reinforced Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 166 MPa | 24100 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 633 Nylon 6/6, Glass Reinforced, Flow Enhanced, UL Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |