Polymer Property : Tensile Strength, Ultimate = 235 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1.62 MPa
235 psi
Valley Adhesives EM-120 High Performance Application Glue Stick
Valley Adhesives EM-120 High Performance Application Glue StickGeneral purpose hot melt spray adhesive; High performance and heat resistance with excellent adhesion, shear, peel and high initial str..