Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 161 MPa
23400 psi
5 mm/min
Arkema Group Rilsan® ASR 30 Nylon 12, 30% Carbon Fiber Filled (Dry)
Designation ISO 1874-PA12,M,16-120,CF30Rigid grade with carbon fiber filler (30%) for injection molding. Available color: black.Very high rigidity. High strength-to-weight ratio. Very low shrinkage:..
Tensile Strength, Ultimate 161 MPa
23400 psi
ISO value at 5mm/min.
BASF Capron® 8232G HS BK-102 25% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8232G HS BK-102 is a pigmented black, heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional..