Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2300 MPa | 334000 psi | |
China Tungsten YG4C Tungsten Carbide Information provided by China Tungsten |
|||
Tensile Strength, Ultimate | 2300 MPa | 334000 psi | |
China Tungsten YG9 Tungsten Carbide Powder Information provided by China Tungsten |
|||
Tensile Strength, Ultimate | 2300 MPa @Temperature 23.0 °C |
334000 psi @Temperature 73.4 °F |
|
Assab Steels HOTVAR Hot Work Steel HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue.. |