Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1580 MPa | 229000 psi | |
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core Description: Ferrium® C64™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the .. |
|||
Tensile Strength, Ultimate | 1580 - 1590 MPa | 229000 - 230000 psi | |
Latrobe Lescalloy® HP 9-4-30 VAC-ARC ; 13.5 in RCS Billet Size High Strength Alloy Steel LESCALLOY HP 9-4-30 VAC-ARC steel is a low alloy, high strength steel with a high nickel and cobalt content to promote toughness. The alloy has been designed to have high hardenability, good weldabi.. |
|||
Tensile Strength, Ultimate | 1580 MPa | 229000 psi | Tempering Temperature- 600°F |
Crucible Steel 422 Stainless Steel Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is.. |