Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 2280 MPa | 331000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |