Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 156 MPa
22600 psi
ASTM D638
Firestone CG430-203 Nylon 6, 30% Fiberglass Filled
Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone
Tensile Strength, Ultimate 156 MPa
22600 psi
Shinil Chemical SHINSTRA PA-6 AG30N Structural Polymer Wheel Cover
SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog..
Copyright © lookpolymers.com All Rights Reserved