Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1483 MPa | 215100 psi | |
ATI Allvac® Nickelvac® D6AC UNS K24728 Specialty Steel Uses: High performance aircraft structural parts.Property values are for samples in the metallurgical condition: 1550°F Q + 1000°F T.Information provided by Allvac, An Allegheny Teledyne Company. |
|||
Tensile Strength, Ultimate | 1483 MPa | 215100 psi | |
ATI Allvac® Vasco® 13-8Mo Precipitation Hardening Steel, Heat Treatment: 927°C (1700°F) + Age Data provided by Allvac.Applications: Airframe structurals, missile components, valve parts, fasteners, chemical process equipment. |
|||
Tensile Strength, Ultimate | 1483 MPa | 215100 psi | |
ATI Allvac® Vasco® D6AC Specialty Steel, Heat Treatment: 913°C (1675°F) Q+T Data provided by Allvac.Applications: High performance aircraft structural parts. |