Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 21.13 MPa | 3065 psi | s.d. 1.72 MPa, test specimen 1.20 cm wide (s.d. 0.003 cm), 0.23 cm thick (s.d. 0.010 cm) |
Schmelzer Industries Pearlveil 110-10 Fiberglass Veil Economical alternative for flat or shallow applications. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. Data provided by the manufacturer, Schmel.. |