Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 14.31 MPa | 2075 psi | ASTM D638 |
Colorite Polymers MULTICHEM™ 7514 Vinyl-Urethane Blend Description: MULTICHEM™ is characterized by:Greater ResiliencyImproved ElasticityLow Temperature PropertiesLower ExtractabilityMolding and ExtrusionInformation provided by Colorite Polymers. |