Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 2020 MPa
293000 psi
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications
Description: Ferrium® M54™ is an ultra high-strength steel for structural applications. Ferrium® M54™ was designed to provide mechanical properties equal to, or better than ultrahigh-strength st..