Polymer Property : Tensile Strength, Ultimate = 201 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 201 MPa
29200 psi
ASTM D638
A. Schulman ComAlloy Hiloy® 634 Nylon 6/6, Glass Reinforced, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company.43% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.