Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 196.5 MPa | 28500 psi | |
IBC Advanced Alloys Beralcast® 191 Beryllium-Aluminum Alloy This alloy consists of 65% Be and 35% Al (by weight) and is used primarily for moderate strength cast electronic and thermal packaging applications. BeAl-191 also provides a unique capability for se.. |