Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 194000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1340 - 1590 MPa
194000 - 231000 psi
Materion Beryllium Copper Alloy 25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17200)
Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it..
Tensile Strength, Ultimate 1340 - 1590 MPa
194000 - 231000 psi
Materion Beryllium Copper Alloy M25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17300)
Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it..
Tensile Strength, Ultimate 1340 MPa
194000 psi
Haynes 214® alloy, 30% cold reduction
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Ultimate 1340 MPa
194000 psi
Haynes 242® alloy, after 1000 hours exposure at 650°C (1200°F)
Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm..
Copyright © lookpolymers.com All Rights Reserved