Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 131.9 MPa
19130 psi
ISO 527-1, 2
Polyplastics Duranex® CRN7030 Polybutylene Terephthalate (PBT), Low gas generation, Low contact contamination, FR, UL approved regrind 50%, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..