Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 19.00 MPa | 2756 psi | ASTM D638 |
Ecomass® 720ZC85 Stainless Steel Filled ABS High Specific GravityStainless Steel Powder Filled ABSGood ToughnessPlateableInformation provided by Technical Polymers |