Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1300 MPa | 188000 psi | |
Latrobe Lescalloy® Jethete M-152 ESR 1.5" RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
Tensile Strength, Ultimate | 1300 - 1300 MPa | 188000 - 189000 psi | |
Latrobe Lescalloy® Jethete M-152 ESR 1.25 RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |