Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1870 MPa
271000 psi
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..