Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.5 - 184 MPa

@Temperature -40.0 - 150 °C
2970 - 26700 psi

@Temperature -40.0 - 302 °F
Average value: 78.5 MPa Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Tensile Strength, Ultimate 20.5 - 184 MPa

@Strain 0.230 - 10.5 %
2970 - 26700 psi

@Strain 0.230 - 10.5 %
Average value: 78.5 MPa Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..