Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 124 MPa | 17900 psi | 5mm/min; ASTM D638 |
Asia International Enterprise (Hong Kong) 60G2-13GF Nylon 66, 13% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |