Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 12.1 MPa
1750 psi
Sylvin Technologies 8940-70 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 12.1 MPa
1750 psi
Sylvin Technologies 9940-70 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 12.1 MPa
1750 psi
Sylvin Technologies 9960-90 Natural PVC Molding Compound
Information provided by Sylvin Technologies Inc.
Tensile Strength, Ultimate 12.1 MPa
1750 psi
Dow Corning SILASTIC® LS 5-2040 FLUOROSILICONE RUBBER
40 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning
Tensile Strength, Ultimate 12.1 MPa
1750 psi
ASTM D412
BCC Products BC 8990 Polyurethane Elastomer
BC8990 is a two-component urethane elastomer compound specifically designed for general purpose molding and casting of various shapes. This product is a safe, easy-to-handle, room temperature mixing..
Tensile Strength, Ultimate 12.1 MPa
1750 psi
ASTM D638
Colorite Polymers 6577 Non-Phthalate 77 Series Vinyl Compound
Description: The Colorite 77 series is a family of compounds designed for those medical device producers that require the use of a non-phthalate plasticizer that has superior resistance to extractio..
Tensile Strength, Ultimate 12.1 MPa
1750 psi
ASTM D638
Colorite Polymers 7075 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 12.1 MPa
1750 psi
Sylvin Technologies 9812A-80 Natural PVC for Injection Molding
Information provided by Sylvin Technologies Inc.