Polymer Property : Tensile Strength, Ultimate = 170000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 689 - 1170 MPa
100000 - 170000 psi
Meehanite Ductliron® SH-100 Nodular Graphite Ductile Iron
Type SP-100 is characterized by its exceptional hardenability. It is particularly suited where high strengths are desired in relatively heavy casting sections. In the as-cast condition it has a pe..