Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 11.6 MPa
1680 psi
ASTM D638
Multibase Multi-Flex® TPE G 7455 X
Multi-Flex® G 7455 X is based on the Kraton G 78455 X formulation. It has low specific gravity as well as having a UL 94 rating of V-0. Ash is 5.2%. Multi-Flex TPE contains Kraton™ G.Data provi..
Tensile Strength, Ultimate 11.6 MPa
1680 psi
TPE-0153 (ASTM D 412)
Advanced Elastomer Systems Santoprene® 153-38 Thermoplastic Rubber  (discontinued **)
A black thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can be pr..
Tensile Strength, Ultimate 11.6 MPa
1680 psi
ASTM D638
Colorite Polymers 6533 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
Tensile Strength, Ultimate 11.6 MPa
1680 psi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Advanced Polymer Alloys Alcryn® 4680 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Tensile Strength, Ultimate 11.6 MPa
1680 psi
ASTM D412-75
3M SJ-1FB Cold Shrink Foldback Splice Jacket Kits
3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice..
Tensile Strength, Ultimate 11.6 MPa
1680 psi
ASTM D412-75
3M SJ-2FB Cold Shrink Foldback Splice Jacket Kits
3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice..
Tensile Strength, Ultimate 11.6 MPa
1680 psi
ASTM D412-75
3M SJ-3FB Cold Shrink Foldback Splice Jacket Kits
3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice..
Tensile Strength, Ultimate 11.6 MPa
1680 psi
ASTM D412-75
3M SJ-4FB Cold Shrink Foldback Splice Jacket Kits
3M Cold Shrink Foldback Splice Jacket Kits SJ-FB Series are a series of fold back, tubular rubber sleeve that combined with Scotch® Rubber Mastic Tape 2228 provide a sealed jacket over cable splice..