Polymer Property : Tensile Strength, Ultimate = 16710 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 115.2 MPa
16710 psi
ASTM D638
Plenco 51240 PET, Pellet, Injection Molded, Green  (discontinued **)
PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P..