Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 1137 MPa | >= 164900 psi | |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to |