Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1125 MPa | 163200 psi | |
Haynes 25 alloy, room temperature after 10% cold reduction, 1065°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |