Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 163 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 163 MPa

@Temperature 260 °C
23600 psi

@Temperature 500 °F
Copper butt joint
Lucas-Milhaupt SIL-FOS 5 Silver/ Copper/ Phosphorus Alloy
Applications: Sil-Fos 5 was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditionin..
Tensile Strength, Ultimate 163 MPa

@Temperature 260 °C
23600 psi

@Temperature 500 °F
Copper butt joint
Lucas-Milhaupt SIL-FOS Silver/ Copper/ Phosphorus Alloy
Applications: Sil-Fos was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditioning ..
Tensile Strength, Ultimate 163 MPa
23600 psi
ASTM D638
A. Schulman ComAlloy Lubrilon® 629 Nylon 6/6, Glass Fiber/PTFE Filled, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..