Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1583 MPa | 229600 psi | Hardened 1900°F, Tempered 550°F |
ATI Allegheny Ludlum 420 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Ultimate | 1583 MPa | 229600 psi | Typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 288°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |