Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.76 MPa
1561 psi
Freudenberg Simrit V160 Non-Black Compound
Specific compounding ingredients can reduce or eliminate the presence of carbon black. These compounds may provide improved resistance to oxidative environments and reactive plasmas. The inorganic p..