Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1020 MPa
148000 psi
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 12.7 mm (1/2 in.) thick plate
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Tensile Strength, Ultimate 1020 MPa
148000 psi
Industeel Superplast® SP300 Prehardened Mold Steel
Superplast® 300 (SP300) is a prehardened steel with a BHN 300 (32 HRC) to be used for plastic injection molds, extrusion dies, and compression molds offering improved performance for the mold mak..
Tensile Strength, Ultimate 1020 MPa
148000 psi
Haynes 214® alloy, 50% cold reduction, 1095°C (2000°F) for 5 minutes
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Tensile Strength, Ultimate 1020 MPa
148000 psi
Haynes Ultimet® alloy, 6.3-38.1 mm plate
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Tensile Strength, Ultimate 1020 MPa
148000 psi
Haynes Ultimet® alloy, aged 1000 hours at 204°C (400°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Tensile Strength, Ultimate 1020 MPa
148000 psi
Haynes Ultimet® alloy, mill annealed
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Tensile Strength, Ultimate 1020 MPa
148000 psi
Haynes 188 alloy, plate at RT after 8000 hours at 760°C (1400°F)
Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr..
Tensile Strength, Ultimate 1020 MPa
148000 psi
Typical
TIMET 8-1-1 Titanium Alloy (Ti-8Al-1Mo-1V); Annealed Sheet
Industry Specifications: USA Aerospace: AMS 4915,4916. France: T-A8DV. Features: Designed for creep resistance up to 450°C, used primarily in engine applications such as forged compressor blades..
Tensile Strength, Ultimate 1020 MPa
148000 psi
Elgiloy® Co-Cr-Ni Alloy, Strip, 10% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..
Tensile Strength, Ultimate 1020 MPa

@Temperature 199 °C
148000 psi

@Temperature 390 °F
(hardened to 350 HB)
Bohler-Uddeholm BÖHLER RAMAX® HH Modified 420F
Chromium alloyed steelTypical applications for Ramax® HH are: holders and bolsters for plastic molds, plastic and rubber molds with low requirements on polishability, and dies for plastic extrusion..
Tensile Strength, Ultimate 1020 MPa

@Thickness 4.762 mm
148000 psi

@Thickness 0.1875 in
Typical for Plate, 1/4-Hard, Longitudinal
AK Steel NITRONIC® 30 Austenitic Stainless Steel
AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi..
Tensile Strength, Ultimate 1020 MPa
148000 psi
Average Annealed
ATI Allegheny Ludlum K12® Dual Hardness Steel
This is a roll bonded, dual hardness armor plate consisting of a high hardness front side to break up or flatten incoming projectiles while the back side functions to capture the projectile.The comp..
Tensile Strength, Ultimate 1020 MPa
148000 psi
Haynes 25 alloy, room temperature after 10% cold reduction, 1175°C anneal for 5 minutes
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall..
Tensile Strength, Ultimate 1020 MPa
148000 psi
Haynes 230® alloy, 50% cold reduction, 1066°C anneal for 5 minutes
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..